Compressive Strength |
||
ASTM C-109 |
7 days |
4000 psi |
28 days |
5500 psi |
|
Flexural Strength |
||
ASTM C-78 |
7 days |
1000 psi |
Tensile Strength |
||
ASTM C-496 |
7 days |
500 psi |
Add approximately 130 pounds ASTM C-33 Concrete sand to each 50 lb bag of FX-285. Use normal dry process shotcrete methods. Be certain receiving surfaces are sound and clean. Predampen surface with clean water for good bond. Follow practices of ACI 506-R85 "Guide to Shotcrete". Mortar should be of plastic consistency when applied whether by shotcrete machinery or by hand.
Proper curing is extremely important and should be conducted in accordance with ACI 308 "Standard Practice for Curing Concrete". Apply a curing compound that complies with the moisture retention requirements of ASTM C 309 such as FX-15 WB curing compound; or moist cure for a minimum of 7 days.
FX-285 is packaged in 50 lb. bags. Each bag yields approximately 1.43 cubic feet when mixed with 130 lbs of ASTM C-33 sand and 2.5 gallons of potable water is added.
WARNING! CONTAINS FREE SILICA & PORTLAND CEMENT. DO NOT BREATHE DUST. May cause delayed lung injury (silicosis). Follow O.S.H.A. safety and health standards for crystalline silica (quartz). Cement powder or freshly mixed concrete, grout or mortar may cause skin injury. Avoid contact with skin and wash exposed skin areas promptly with water. If any cement powder or mixture gets into the eyes, rinse immediately and repeatedly with water and get prompt medical attention.